Caution!

Visiting this web site requires a newer version of Netscape Communicator.

Visit Microsoft's Web site to obtain the newest version of Internet Explorer, or visit Netscape's Web site to obtain the newest version of Netscape Communicator.

Visiting this web site without first upgrading your browser may result in unreliable behavior.













COMPANY



Home


Contact Us


Services/Finishes


Links


Articles


Company History


Policies


FAQ


Customer Approvals


Sitemap





  Quality Plating Co., Inc.

801-355-7424  

sales@qualityplating.com  




Frequently Asked Questions

If your questions are not answered on the web site, please feel free to contact us.


previous
index
view all
next

How much build-up will I have?

Electroplating typically has build-up of less than 0.001", but this can vary according to process parameters. Additional information relating to individual coating thickness can be found under the "Services" heading of each individual finish.

Surface treatments like chemical conversion coatings on aluminum, black oxide, and Dow #7 have no build-up.

Electroless plating such as electroless nickel has the ability to hold tolerances as close as 0.0002".

Coating thickness of electrolytic processes like chrome and nickel plating are more difficult to control since they build up more on outside corners and edges (which are high current density areas) than on inside corners, recessed areas and center areas (which are low current density areas). If your tolerances are closer than 0.005", it would be wise to contact us for advice.